Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 45.5 MPa | 6600 psi | Steel-Steel; after optimum cure |
Armstrong A-12-T Epoxy Adhesive Provides the same basic properties as A-12, but in thixotropic, non-sag, easily-brushable paste form. An ideal material for use where adhesive flow during cure cannot be tolerated. A-12-T meets t.. |