Polymer Property : Adhesive Bond Strength = 4450 psi
Polymer Property :
Adhesive Bond Strength =
4450 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Adhesive Bond Strength
30.7
MPa
4450
psi
Steel-Steel; after optimum cure
Armstrong X-81-A/F Epoxy Adhesive
Information provided by Ellsworth Adhesives.