Adhesive Bond Strength 0.600 - 29.0 MPa
87.0 - 4200 psi
Average value: 19.5 MPa Grade Count:23
Overview of materials for Methacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri..