Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.241 MPa
35.0 psi
Aluminum; Lap Shear, cured 21 days, 22°C; 50% RH; 0.5 mm gap; ISO 4587
Loctite® 5920™ RTV Silicone Sealant
LOCTITE® 5920™ is a moisture-curing, non-corrosive silicone. The thixotropic nature of LOCTITE® 5920™ reduces the migration of liquid product after application to the substrate. It has been desi..
Adhesive Bond Strength 0.241 MPa
35.0 psi
Mild Steel; Lap Shear, cured 21 days, 22°C; 50% RH; 0.5 mm gap; ISO 4587
Loctite® 5920™ RTV Silicone Sealant
LOCTITE® 5920™ is a moisture-curing, non-corrosive silicone. The thixotropic nature of LOCTITE® 5920™ reduces the migration of liquid product after application to the substrate. It has been desi..
Adhesive Bond Strength 0.241 MPa
35.0 psi
Stainless Steel; Lap Shear, cured 21 days, 22°C; 50% RH; 0.5 mm gap; ISO 4587
Loctite® 5920™ RTV Silicone Sealant
LOCTITE® 5920™ is a moisture-curing, non-corrosive silicone. The thixotropic nature of LOCTITE® 5920™ reduces the migration of liquid product after application to the substrate. It has been desi..