Mechanical Properties Metric English Comments
Adhesive Bond Strength 2.28 MPa
330 psi
ASTM-D4541
Abatron Acrylic 57-1™ Clear, Water-Based Coating
Acrylic 57-1™ is a high-gloss, non-yellowing acrylic coating. It forms a very clear film with exceptional mar resistance. Because it will not yellow and is stain resistant, it is an excellent choic..