Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 3.79 - 4.17 MPa
550 - 605 psi
Sika Industry SikaFlex 255FC Fast Cure One Part Polyurethane Adhesive
Sika 255FC SikaFlex Fast Cure One Part Polyurethane AdhesiveThis is a fast curing flexible high performance polyurethane adhesive for bonding glass to metal surfaces. Initial strength is derived fro..
Adhesive Bond Strength 3.79 MPa
550 psi
Nitrile-Nitrile; Substrate Failure; Tensile Lap Shear
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate
Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver..
Adhesive Bond Strength 3.79 MPa
550 psi
Lap shear, alum to alum
Tra-Con Tra-Bond 957-1R Polyurethane Adhesive
TRA-BOND 957-1R is a polyurethane compound used on stress sensitive components and encapsulation applications. Information provided by Tra-Con Inc.