Polymer Property : Adhesive Bond Strength = 3.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 3.10 MPa
450 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Resinlab® EP1385 Black Epoxy Formulation
Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w..
Adhesive Bond Strength 3.10 MPa
450 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Resinlab® EP1385 Clear Epoxy Formulation
Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w..
Adhesive Bond Strength 3.10 - 44.8 MPa
450 - 6500 psi
Average value: 13.0 MPa Grade Count:32
Overview of materials for Epoxy Encapsulant, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o..
Adhesive Bond Strength 3.10 MPa
450 psi
Lap shear, steel to steel
Momentive Performance Materials LVG342 Low Volatile Silicone Adhesive, Mixed, White
LVG342 low volatile silicone adhesive is a two component, thixotropic silicone adhesive that cures very quickly at elevated temperatures to a durable elastomer. LV342 was specifically developed for..