Polymer Property : Adhesive Bond Strength = 2926 psi
Polymer Property :
Adhesive Bond Strength =
2926 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Adhesive Bond Strength
20.17
MPa
2926
psi
Lap shear, alum to alum, 30 min @ 120°C
Tra-Con Tra-Duct 921H01
Information provided by Tra-Con Inc.