Polymer Property : Adhesive Bond Strength = 29.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength >= 0.200 MPa
>= 29.0 psi
on metals
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength >= 0.200 MPa
>= 29.0 psi
on wood
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength >= 0.200 MPa
>= 29.0 psi
on plastic
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength >= 0.200 MPa
>= 29.0 psi
on metals
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength >= 0.200 MPa
>= 29.0 psi
on wood
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength >= 0.200 MPa
>= 29.0 psi
on plastic
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength >= 0.200 MPa
>= 29.0 psi
on metals
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength >= 0.200 MPa
>= 29.0 psi
on wood
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength >= 0.200 MPa
>= 29.0 psi
on metals
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength >= 0.200 MPa
>= 29.0 psi
on wood
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength >= 0.200 MPa
>= 29.0 psi
on plastic
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength 0.200 - 0.400 MPa
29.0 - 58.0 psi
on concrete; DIN EN 1607
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..