Polymer Property : Adhesive Bond Strength = 25.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 25.9 MPa

@Temperature 25.0 °C
3750 psi

@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
Armstrong A-34 Epoxy Adhesive
This white paste material is a fast-curing adhesive with a working life of 20-25 minutes in a 100-gram mass. Mixing ratio is a convenient 1:1. A-34 has excellent wetting properties and is suggeste..
Adhesive Bond Strength 25.9 MPa
3750 psi
Grit blasted steel
Loctite® Black Max® 380 Instant Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..