Polymer Property : Adhesive Bond Strength = 2385 psi
Polymer Property :
Adhesive Bond Strength =
2385 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Adhesive Bond Strength
16.44
MPa
2385
psi
tensile shear; ASTM D1002
ITW Devcon Metal Repair Stainless Steel Putty (ST), Grey
Information provided by ITW Devcon