Polymer Property : Adhesive Bond Strength = 2026 psi
Polymer Property :
Adhesive Bond Strength =
2026 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Adhesive Bond Strength
13.97
MPa
2026
psi
tensile shear; ASTM D1002
ITW Devcon Plastic Steel® Metal Repair 5 Minute® Putty (SF), Dark Grey
Information provided by ITW Devcon