Polymer Property : Adhesive Bond Strength = 2.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 2.10 MPa
305 psi
EPDM, Substrate Failure, Shear; ASTM D1002
Permabond 930 Cyanoacrylate
PERMABOND 930 is a low odor, non­fogging, non­frosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The ..
Adhesive Bond Strength 2.10 MPa
305 psi
EPDM, Substrate Failure, Shear; ASTM D1002
Permabond 931 Cyanoacrylate
PERMABOND 931 is a low odor, non­fogging, non­frosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv..
Adhesive Bond Strength 2.10 MPa
305 psi
EPDM, Substrate Failure, Shear; ASTM D1002
Permabond 932 Cyanoacrylate
PERMABOND 932 is a low odor, non­fogging, non­frosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv..
Adhesive Bond Strength 2.10 MPa
305 psi
EPDM, Substrate Failure, Shear; ASTM D1002
Permabond 935 Cyanoacrylate
The PERMABOND 930 series is a family of low odor, non-fogging, non-frosting cyanoacrylates. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyano..