Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 2.0594 MPa | 298.69 psi | At 100% cohesive failure |
Momentive Performance Materials RTV142 White, Low Volatile, One Component Silicone Sealant RTV 142 one-component, ready-to-use adhesive sealant cures to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Methyl alcohol vapors are released.. |