Polymer Property : Adhesive Bond Strength = 19.9 MPa
Polymer Property :
Adhesive Bond Strength =
19.9 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Adhesive Bond Strength
19.9
MPa
2890
psi
Adhesive tensile shear strength; ASTM D1002
Devcon Tile Adhesive Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.