Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 1.1768 MPa | 170.68 psi | At 100% cohesive failure |
Momentive Performance Materials RTV133 Black, Flame Retardant, One Component Silicone Sealant RTV 133 black, one-component, ready-to-use rubber adhesive sealant is recommended for evaluation in applications in the electronic, aerospace, appliance, transportation and other industries where re.. |