Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.0103 - 150 MPa
1.50 - 21800 psi
Average value: 3.62 MPa Grade Count:40
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..