Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 15.5 MPa | 2250 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
ITW Devcon 2 Ton® Epoxy Clear Epoxy, Clear, White Information provided by ITW Devcon |
|||
Adhesive Bond Strength | 15.5 MPa | 2250 psi | lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002 |
ITW Devcon Composite Welderâ„¢ Methacrylate Adhesive FS, Blue Green, Black Information provided by ITW Devcon |
|||
Adhesive Bond Strength | 15.5 MPa @Temperature -54.4 °C |
2250 psi @Temperature -66.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong C-4/D Epoxy Adhesive A low viscosity, clear amber, unfilled adhesive, recommended for use with activators D or W. C-4 with Activator W offers maximum versatility in that differing degrees of flexibility can be achieved .. |
|||
Adhesive Bond Strength | 15.5 MPa | 2250 psi | Lap shear, alum to alum, 24 hrs @ 25°C |
Tra-Con Tra-Bond 2138 Easy-Flow No-Sag Epoxy Adhesive TRA-BOND 2138 epoxy adhesive is an easy-to-apply, room temperature cure epoxy adhesive system developed for structural bonding applications on vertical or overhead surfaces where its instant develop.. |