Polymer Property : Adhesive Bond Strength = 141 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.970 MPa
141 psi
Typical lap shear
Momentive Performance Materials IS803 Black Adhesive Sealant, General Purpose Paste
One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: Use for general purpose,..
Adhesive Bond Strength 0.970 MPa
141 psi
Typical lap shear
Momentive Performance Materials IS808 Translucent Adhesive Sealant, General Purpose Paste
One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: Use for general purpose,..
Adhesive Bond Strength 0.970 MPa
141 psi
Typical lap shear
Momentive Performance Materials IS802 White Adhesive Sealant, General Purpose Paste
One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: Use for general purpose,..