Polymer Property : Adhesive Bond Strength = 13.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 13.7 MPa
1980 psi
Aluminum-Aluminum; Tensile Lap Shear
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate
Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver..
Adhesive Bond Strength 13.7 MPa
1980 psi
Lap shear, alum to alum
Tra-Con Tra-Bond 2230 Color Keyed, High Temperature Epoxy Adhesive
TRA-BOND 2230 is a clear, low viscosity, high temperature, two-part epoxy adhesive that changes colors during the curing process to indicate cure status. The unmixed components are light yellow; the..
Adhesive Bond Strength 13.7 MPa
1980 psi
Lap shear, alum to alum
Tra-Con Tra-Bond F230 Color Keyed High Temperature Epoxy Adhesive
TRA-BOND F230 is a clear, low viscosity, high temperature, two-part epoxy adhesive that changes colors during the curing process to indicate cure status. The unmixed components are light yellow; the..