Mechanical Properties Metric English Comments
Adhesive Bond Strength 12.7 MPa
1840 psi
Chromium-Chromium; Tensile Lap Shear
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate
Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver..