Mechanical Properties Metric English Comments
Adhesive Bond Strength 7.50 MPa
1090 psi
2 Day Cure; ASTM C882
Protective Coating PC-Concrete™ Epoxy Concrete Anchoring and Repair System
PC Concrete™ epoxy gel is an anchoring and concrete repair product. PC Concrete™ is formulated for anchoring threaded rods, bolts, rebar dowels and smooth dowels into concrete, grout filled block,..