Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 10.3 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.0710 MPa
10.3 psi
Arlon SQA-TMS-011
Arlon 56946C026 Silicone Rubber/Fiberglass Laminate
Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene
Copyright © lookpolymers.com All Rights Reserved