Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 0.890 MPa | 129 psi | Lap Shear vs. aluminum or glass |
Momentive Performance Materials IGS3723 Insulating Glass Sealant Two-component silicone which cures to form a high strength, high modulus sealant with excellent adhesion to glass. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Silicones becam.. |