Polymer Property : Adhesive Bond Strength = 0.100 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.100 - 0.400 MPa
14.5 - 58.0 psi
Average value: 0.165 MPa Grade Count:5
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on concrete
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on mineralic surfaces
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on gluing mortar
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on plasters
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on concrete
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on mineralic surfaces
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on gluing mortar
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on plasters
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on concrete
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on mineralic surfaces
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on gluing mortar
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on plasters
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength 0.100 - 0.400 MPa
14.5 - 58.0 psi
Average value: 0.165 MPa Grade Count:5
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on concrete
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on mineralic surfaces
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on gluing mortar
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength <= 0.100 MPa
<= 14.5 psi
on plasters
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength 0.100 - 0.200 MPa
14.5 - 29.0 psi
on plasters
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..