Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 0.0152 MPa | 2.20 psi | MIL-I-46852C |
Arlon R3792-920-10R##-P0 Silicone Rubber This self-fusible silicone tape is specially formulated to yield improved flexibility, elongation and elastic recovery at low operating temperature (-70°C to -100°C) where standard fusible silicon.. |