Mechanical Properties Metric English Comments
Tangent Modulus 179 MPa
26000 psi
T.D.; ASTM D882
Eastman Eastman AP005 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..