Tangent Modulus 880 MPa
128000 psi
ASTM D790
Flint Hills P5M2Z-012 Polypropylene Random Copolymer
Features: Good contact clarity. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: film and blow moldingInformation Provided by Flint Hills Resources