Mechanical Properties Metric English Comments
Tangent Modulus 1104 MPa
160100 psi
ASTM D790
Flint Hills AP6835-HS Polypropylene Impact Copolymer
Features: Excellent processing, good low temperature impact strength.Applications: Injection molding: Appliance components, consumer durables and closuresInformation Provided by Flint Hills Resource..