2% Secant Modulus 0.572 GPa
83.0 ksi
0.5"/min; ASTM D790
LyondellBasell Petrothene® GA594189 Linear Low Density Polyethylene, Injection Molding Grade
PETROTHENE GA594189 is a pelletized LLDPE copolymer resin for injection molding thin-walled items requiring high flow and short cycle times. GA594189 exhibits excellent flow, warp resistance and sur..