Polymer Property : 2% Secant Modulus = 35.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
2% Secant Modulus 0.241 GPa
35.0 ksi
Procedure A; ASTM D882
3M SMS Heat Shrink Tubing
3M Heat Shrink Tubing SMS is a co-extruded, dual wall product. It is a composite of a polyolefin shrinkable outer wall and a thermoplastic adhesive inner wall. SMS tubing does not degrade when expos..