Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.0258 GPa | 3.74 ksi | ASTM D790 |
Dow Engage® 8401 Polyolefin Elastomer Description: Engage® 8401 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable, flexible injection molded industrial and consumer goods. Engage® 8401 pr.. |