Polymer Property : 2% Secant Modulus = 28.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
2% Secant Modulus 0.193 GPa
28.0 ksi
12.7mm/min; ASTM D790
Westlake EC1390AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC1390 is used primarily in extrusion-coating applications that require fast line speeds and relatively low coating weights. When compared with other low-density po..