Mechanical Properties Metric English Comments
2% Secant Modulus 0.186 GPa
27.0 ksi
Crosshead Speed - 1/2 in/min; ASTM D790
LyondellBasell Petrothene® NA870252 Low Density Polyethylene
ApplicationsPETROTHENE NA 870-252 exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include caps and closures, housewares, toys, co..
2% Secant Modulus 0.186 GPa
27.0 ksi
3M MW Heat Shrink Tubing
3M Heat Shrink Tubing MW is a semi-rigid, 110°C heat-shrinkable polyolefin tubing that is a co-extruded and selectively cross-linked to provide an integral, meltable inner wall. When heated in exce..