2% Secant Modulus 0.125 GPa
18.1 ksi
TD; ASTM D882
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene
09X02 is a high performance LLDPE (HP-LLDPE) cast film grade combines ease of processing with low gels and good film strength. Its excellent stretchability makes this grade particularly suited for s..