Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
2% Secant Modulus 0.834 GPa
121 ksi
Crosshead speed - 0.5" min; ASTM D790
LyondellBasell Alathon® M4621 High Density Polyethylene
ApplicationsALATHON M 4621 is a copolymer that provides outstanding stress crack resistance and low temperature impact strength. Typical applications include small two-piece engine gas tanks, waste..