Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.0136 GPa | 1.97 ksi | ASTM D790 |
Dow Engage® 8100 Polyolefin Elastomer Description: Engage® 8100 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide range of general purpose thermoplastic elastomer ap.. |
|||
2% Secant Modulus | 0.0136 GPa | 1.97 ksi | ASTM D790 |
Dow Engage® 8107 Polyolefin Elastomer Description: Engage® 8107 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio.. |