Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 1.29 GPa | 187 ksi | Crosshead speed - 0.5" min; ASTM D790 |
LyondellBasell Alathon® M6580 High Density Polyethylene ApplicationsALATHON M 6580 is a narrow molecular weight distribution homopolymer that enhances processability and stiffness, exhibits excellent color, low odor and good processing stability. Typica.. |