Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 1.08 GPa | 157 ksi | Crosshead speed - 0.5" min; ASTM D790 |
LyondellBasell Alathon® M5562 High Density Polyethylene ApplicationsALATHON M 5562 is a copolymer with medium molecular weight distribution. This resin provides moderate stiffness, toughness and stress crack resistance. Typical applications include noz.. |
|||
2% Secant Modulus | 1.08 GPa | 156 ksi | Crosshead speed - 0.5" min; ASTM D790 |
LyondellBasell Alathon® M5350 High Density Polyethylene ApplicationsALATHON M 5350 copolymer with narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing s.. |