Mechanical Properties Metric English Comments
2% Secant Modulus 1.04 GPa
151 ksi
Crosshead speed - 0.5" min; ASTM D790
LyondellBasell Alathon® H5520 High Density Polyethylene
ApplicationsALATHON H 5520 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include house..
2% Secant Modulus 1.04 GPa
151 ksi
Crosshead Speed 0.5 in/min; ASTM D790
LyondellBasell Alathon® M5363 High Density Polyethylene
ApplicationsALATHON L 4912 is a high molecular weight, high density copolymer with a broad molecular weight distribution. This resin provides excellent stiffness and a good balance of film properti..
2% Secant Modulus 1.04 GPa
151 ksi
Crosshead speed - 0.5" min; ASTM D790
LyondellBasell Alathon® M5370 High Density Polyethylene
ApplicationsALATHON M 5370 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processability. Typic..
2% Secant Modulus 1.04 GPa
151 ksi
ASTM D790
LyondellBasell Alathon® M5370PX High Density Polyethylene, Extrusion Grade
ALATHON M5370PX is a copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processability. T..