Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 1.01 GPa | 146 ksi | ASTM D790 |
LyondellBasell Alathon® L4904 High Density Polyethylene, Pipe and Sheet Extrusion Grade Alathon L4904 is a bimodal, high molecular weight, high density polyethylene resin with excellent processability characteristics that meet the high performance requirements of demanding pressure pip.. |
|||
2% Secant Modulus | 1.01 GPa | 147 ksi | ASTM D790 |