Polymer Property : 2% Secant Modulus = 0.703 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
2% Secant Modulus 0.703 GPa
102 ksi
TD, 1 in/min; ASTM D882
Total HDPE 6420 High Density Polyethylene, Film Resin
Polyethylene: Medium molecular weight, high density film resinCharacteristics:Excellent moisture barrier propertiesLow gelsLow taste and odorHigh stiffnessGood processabilityGood compatibility with..