Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.221 GPa | 32.1 ksi | 12.7mm/min; ASTM D790 |
Westlake EM184AA Low Density Polyethylene WESTLAKE low-density polyethylene EM184 is a low density injection-molding formulation suggested for the production of closures where a high melt index is needed to meet shrinkage requirements and f.. |
|||
2% Secant Modulus | 0.221 GPa | 32.0 ksi | |
3M TMW Tubing 3M TMW Tubing is a semi-rigid translucent heat-shrinkable polyolefin tubing that is co-extruded and selectively cross-linked with an integral, meltable inner wall. When heated in excess of 135°C th.. |