Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.185 GPa | 26.8 ksi | TD; ASTM D882 |
Iran Petrochemical (PCC) 12XF6 Linear Low Density Polyethylene 12XF6 is a high performance LLDPE (HP-LLDPE) blown film grade for high film strength applications.Information provided by Iran Petrochemical Commercial Co. |