Polymer Property : 2% Secant Modulus = 0.117 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
2% Secant Modulus 0.117 GPa
17.0 ksi
3M EPS-300 Heat Shrink Tubing
3M Heat Shrink tubing EPS-300 is a 3:1 thin-wall, flexible tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with ..