Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.100 GPa | 14.5 ksi | TD; ASTM D882 |
Iran Petrochemical (PCC) LL0220KJ Linear Low Density Polyethylene LL0220KJ are linear low density polyethylene copolymers containing butane-1 as the comonomer.Applications: shipping sacks, carrier and garbage bags, consumer packaging, high clarity film, agricultu.. |