Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.0679 GPa | 9.85 ksi | ASTM D790 |
Dow Engage® ENR 7086.01 Ethylene-Butene Copolymer Description: ENR 7086.01 is a revolutionary new ethylene-butene copolymer with a broader molecular weight distribution and much higher levels of long chain branching than other commercially availabl.. |