Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 99.0 J | 73.0 ft-lb | Hardening Temperature- 1065°C; Tempering Temperature- 595°C |
Crucible Steel CPM® 9V® Tool Steel CPM 9V is made by the Crucible Particle Metallurgy process. Its composition is a modification of CPM 10V with lower carbon and vanadium to improve toughness and heat check resistance. These enhanced.. |