Mechanical Properties Metric English Comments
Charpy Impact 127 J

@Temperature 23.0 °C
93.7 ft-lb

@Temperature 73.4 °F
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Charpy Impact 127 J

@Temperature 23.0 °C
93.7 ft-lb

@Temperature 73.4 °F
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Charpy Impact 127 J

@Temperature 23.0 °C
93.7 ft-lb

@Temperature 73.4 °F
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Charpy Impact 127 J

@Temperature 23.0 °C
93.7 ft-lb

@Temperature 73.4 °F
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Charpy Impact 127 J

@Temperature 23.0 °C
93.7 ft-lb

@Temperature 73.4 °F
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Charpy Impact 127 J

@Temperature 23.0 °C
93.7 ft-lb

@Temperature 73.4 °F
Haynes Ultimet® alloy, all-weld metal, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Charpy Impact 127 J

@Temperature 23.0 °C
93.7 ft-lb

@Temperature 73.4 °F
Haynes Ultimet® alloy, all-weld metal, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Charpy Impact 127 J
93.7 ft-lb
V Notch
Haynes Ultimet® alloy, plate, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Charpy Impact 127 J
93.7 ft-lb
V Notch
Haynes Ultimet® alloy, plate, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..