Mechanical Properties Metric English Comments
Charpy Impact >= 90.0 J
>= 66.4 ft-lb
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24
Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me..
Charpy Impact 90.0 J

@Temperature -50.0 °C
66.4 ft-lb

@Temperature -58.0 °F
Typical
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24
Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me..
Charpy Impact 90.0 J
66.4 ft-lb
V Notch; plate
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Charpy Impact 90.0 J
66.4 ft-lb
Haynes 242® alloy
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Charpy Impact 90.0 J

@Temperature -50.0 °C
66.4 ft-lb

@Temperature -58.0 °F
Typical
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34
Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion..
Charpy Impact >= 90.0 J
>= 66.4 ft-lb
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel
Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom..
Charpy Impact 90.0 J

@Temperature -50.0 °C
66.4 ft-lb

@Temperature -58.0 °F
Typical
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel
Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom..